Amerchol (A subsidiary of The Dow Chemical Company)
A. | |
Water (aqua) | qs |
B. | |
Polyquaternium-67 (SoftCAT SX-400X Polymer (1% aq.), Dow Chemical) | 20.00%w/w |
C. | |
Water (aqua) | qs |
D. | |
Carbomer, 3% aq. (Carbopol 980, Noveon) | 13.55 |
E. | |
Water (aqua) | 23.80 |
F. | |
Cocoamidopropyl betaine (35% solids) | 5.70 |
G. | |
Sodium laureth sulfate (2 moles - 70% solids) | 20.00 |
Tetrasodium EDTA | 0.10 |
H. | |
Triethanolamine | qs |
I. | |
Glycol distearate (and) laureth-4 (and) cocamidopropyl betaine (Euperlan PK 3000 AM, Cognis) | 4.65 |
J. | |
DMDM hydantoin | 0.40 |
K. | |
INCI Not Provided (Dow Corning 2-1310BB Emulsion, 3.30) | qs |
Sodium chloride | 0.50 |
Fragrance (parfum) | qs |
L. | |
Decyl glucoside (50% solids) | 8.00 |
Procedure: Sprinkle B into A at RT with agitation. Allow to disperse completely before beginning to heat slowly. With mixing, heat to 60-65°C. Let cool to RT. Solution should be clear. Set aside. Sprinkle D into C at RT with agitation. Continue mixing until completely dispersed. Do not neutralize. Set aside. In main vessel, combine AB and E. Mix with heating to 70-75°C. Add F. Once uniform, add CD. Continue mixing. In separate vessel, combine G. Heat to 70-75°C, mixing until disolved. Add G to batch with mixing. Adjust pH to 6.0-6.5 with H. Cool to 35-40°C while mixing. Add I and mix until uniform. Add J. Cool to RT. Add K to batch and mix until completely uniform. Adjust to pH 6.0-6.5 using L.